Through hardening — or quench and temper — increases strength, hardness, and toughness across the entire cross-section of a steel component, not just at the surface. Applied to engineering alloys like 4140 and 4340, Q&T delivers the balanced mechanical properties needed for high-stress structural parts, shafts, and fasteners.
Quench and temper is a two-step process. Heating the part above the critical transformation temperature, soaking for the required time to ensure through-thickness temperature uniformity, then quenching rapidly from high temperature, transforming the material to the hard (but brittle) martensitic phase. Tempering follows immediately: a controlled reheat that reduces excess brittleness and restores impact toughness to match your target hardness. Even if maximum hardness is required, a tempering step is always performed at Thermex (albeit at minimum temperature) to reduce some of the quenching stress and restore minimum ductility and toughness.
"*" indicates required fields
The foundational benefits that make Q&T the workhorse process for heavy-duty mechanical components.
Quench-and-temper processing develops consistent core strength and high yield values across the full cross-section of alloys like 4140, 4340, and 4130.
Oil quench on our internal-quench line covers most carbon and alloy steels. Our dedicated pit furnace adds a more aggressive agitated water quench for lean alloys, plus an air-blast quench for air-hardening tool steels like A2, D2, and H13, and 440C martensitic stainless.
Our internal-quench line runs four furnaces sized from 24″ x 36″ x 20″ (750 lb) up to two 36″ x 48″ x 36″ furnaces (2,500 lb each), operating from 1,400-1,750°F. A dedicated pit furnace (27 inches in diameter, 36 inches deep, 1,450-1,850°F operating range) handles alloys that need a more aggressive water or air-blast quench.
Thicker cross-sections respond differently during quenching, which can limit full hardness depth in lower-hardenability alloys. For heavy sections (over 2 inches), 4340 is often preferred over 4140 because its higher hardenability provides for more uniform mechanical properties through thickness.
Sharp internal radii, non-symmetrical wall thicknesses, and unchamfered holes create high stress concentration points during rapid liquid quenching. Adding generous radii and keeping wall transitions gradual drastically reduces the risk of quench cracking.
If your engineering specification calls for tensile or Charpy impact testing, then representative test bars (ideally from the exact same heat as the parts) must be supplied, and will be run with the parts in the same load to allow for confirmation of mechanical properties.
Volumetric expansion occurs when steel transforms to martensite during quenching. Parts grow slightly and may exhibit minor dimensional change depending on geometry. We recommend leaving adequate finish-machining or grinding stock on critical dimensions.
We rack long shafts vertically (up to 34” length) in our furnaces to reduce the tendency to distortion.