Effective November 9th, 2026:

New Trucking Route Around Our Building. View the Route Here

Heat Treating Services

NITROX FNC (ferritic nitrocarburizing) + Post Ox, and Gas Nitriding

Thermex runs two distinct gas-based nitriding processes: Nitrox (FNC + Post Ox), which is the gas-based equivalent to salt bath or liquid nitriding, and conventional 2-stage gas nitriding. Both are lower-temperature (sub-critical) case-hardening surface treatments that suit a wide range of carbon and low-alloy steels, tool steels like H13, and specialty grades such as Nitralloy 135M.

Know the difference

Choosing Between Nitrox and Gas Nitriding

If the part drawing or spec does not dictate which process to use, then service applications often govern the choice:

  • Two-stage Gas Nitriding: Typically used for deeper case depths, diffuses only nitrogen into the surface, and is especially suitable for pre-heat treated alloy steels like 4140, 4340, Nitralloy and tool steels
  • NITROX FNC + Post Ox: Diffuses both nitrogen and carbon for a shallower case in a shorter cycle time, and is suitable for mild and alloy steels. The post-oxidation treatment adds a thin oxide layer for enhanced corrosion resistance and an appealing black matte finish (standard on NITROX; optional at extra cost for gas nitriding).


Most of the time, the application dictates the choice (in the absence of specific instructions or specs for the part). If your part could go either way, send us your print and we can help you choose.

"*" indicates required fields

Name*

Proven Performance

What sets our nitriding lines apart

The advantages that make Nitrox FNC and gas nitriding the practical choice for your parts:

A wear-resistant case

Nitriding builds a hard case in the part’s surface that improves wear and corrosion resistance, as well as fatigue resistance.. Because both processes are performed below the critical phase transformation temperature, no quench is required to obtain the case-hardening effect—delivering exceptional dimensional control.

Consistent results, load after load

Process control at Thermex relies on continuous monitoring and adjustment of the nitriding potential Kn), using hydrogen probes to sample the nitriding atmosphere throughout the entire duration of the process cycle. Routine process verification based on our internal QC testing of Thermex-supplied coupons ensures repeatable and consistent results.

Sized for production parts

Our gas nitriding and Nitrox line runs on two furnaces: a pit-style furnace ( 39 inches in diameter, 72 inches deep, 3,000 lb capacity) and a horizontal furnace (36 inches wide, 48 inches deep, 36 inches high, 3,000 lb capacity).

Practical expertise

Why choose Thermex for nitriding

  • A clean, modern alternative to liquid nitriding

    Gas-based FNC provides precise process atmosphere control without the environmental footprint and salt disposal issues of liquid nitriding, often at a lower unit cost.
  • Dual-furnace redundancy for dependable lead times

    With both horizontal and vertical nitriding furnaces operating in our shop, we maintain process continuity so your job stays on schedule even during furnace maintenance windows.
  • In-house metallurgical verification

    We process test coupons with every load and verify case depth and hardness profiles in our own lab, giving you documented proof on every certificate.

Frequently Asked Questions

Will nitriding alter the dimensional tolerances or thread pitch on finished parts?

Growth is extremely minimal compared to quench processes, but nitriding does form a thin surface compound layer (typically 0.0002″ to 0.0008″ growth per side). For ultra-tight fits or fine precision threads, we recommend discussing pre-machining allowances with our team before final sizing.

Grinding is not recommended because it removes the thin, high-hardness compound layer that imparts wear and corrosion performance. Light polishing or lapping is acceptable if required to achieve specific surface micro-finishes.

Parts must be free of heavy rust, deep scale, paint, severe cutting fluid residues, or plating (like zinc or nickel). Clean, machined and finished bare metal surfaces are required for proper processing.

In almost every case, yes. Gas FNC meets or exceeds the wear and salt-spray corrosion performance of liquid nitriding. Send us your drawing and we’ll help verify if FNC satisfies your print requirements.

Yes. We can mask selected features to prevent nitrogen diffusion during processing — for example keyways, threads, or surfaces reserved for post-heat-treat machining. Share your print with masking requirements called out and we’ll confirm feasibility before quoting. Note that excessive masking can interfere with the nitriding atmosphere – we will review your requirements and advise.

Not yet on our standard nitriding lines — stainless steel isn’t currently supported, though we’re developing a solution. In the meantime, contact our lab team to discuss alternative heat treatment options for your stainless grade.