Carburizing & carbonitriding

Carburizing diffuses carbon into low-carbon mild or alloy steels to build a high hardness, wear-resistant case over a tough core — essential for high-load components like gears, pinions, and drive rings. Carbonitriding modifies this process by adding both carbon and nitrogen, allowing plain low-carbon steels to achieve high surface hardness that standard carburizing alone can’t deliver.

Know the difference

Two Case-hardening Processes, One Shop

While both processes yield a hard outer case over a ductile core, they target different material compositions. Carburizing is optimized for carburizing-grade alloy steels like 8620, 9310, 3312 and 18CrNiMo7-6. Carbonitriding is designed for unalloyed, low-carbon steels like 1018 and 1026 where adding nitrogen increases hardenability in the case. If you’re unsure which process your material requires, send us your print and we’ll point you in the right direction.

"*" indicates required fields

Name*

Carburizing Performance

Case hardening built for wear-critical parts

The performance advantages that make carburizing and carbonitriding high-demand processes for heavy machinery.

Deep, wear-resistant cases

Achieve case depths from 0.010″ up to 0.200″ with surface hardness reaching 62–64 HRC on carburizing grades like 8620, 9310, 4310, 3312 and 18CrNiMo7-6 . Note that for mild steels like 1018 and 1026, case depth is limited to about 0.050” max due to low hardenability of the steel.

Carbonitriding for economical alloys

For parts made from plain low-carbon grades (like 1018 or 1026), carbonitriding delivers a file-hard, wear-resistant surface without requiring more expensive alloy steels—making it a cost-effective solution for high-wear, lighter-load applications.

Sized for production parts

Our internal-quench line runs four furnaces for carburizing: a 24″ wide x 36″ deep x 20″ high furnace at 750 lb, a 30″ x 48″ x 30″ furnace at 2,000 lb, and two 36″ x 48″ x 36″ furnaces at 2,500 lb each. Operating range is 1,400-1,750°F, with an agitated, temperature-controlled oil quench and continuously monitored carbon-potential controlled atmosphere in every furnace.

Quality & capacity

Why choose Thermex for carburizing & carbonitriding

  • Informed spec and drawing reviews

    Drawings and specs are reviewed to ensure that what is being asked for on the drawing and spec can be achieved reliably and consistently. If not, we’ll suggest some possible alternatives.
  • Automated atmosphere & temperature control

    Furnace and quench temperatures, cycle timing, atmosphere carbon potential, gas circulation and quench agitations are continuously monitored and controlled, with all relevant data documented and stored.
  • Multi-furnace capacity and specialty racking

    With multiple furnace lines and specialized racking for a range of part shapes and sizes, we minimize quench distortion and keep production moving on schedule.

Frequently Asked Questions

Can we weld or perform machine modifications on a part after it has been carburized?

Welding directly over a carburized case will cause cracking due to high carbon content in the weld zone. Areas that require post-heat-treat machining or welding must either be masked with stop-off coatings prior to furnace processing or left oversized so the hard case can be turned off before final assembly.

If the case is too shallow or the core is too soft, heavy surface contact loads can crush the underlying core, causing the hard outer shell to spall or collapse (case crushing). We help size effective case depths based on your alloy’s core strength and applied operating loads.

We utilize vertical racking fixtures for shafts up to 34” long to allow for vertical quenching, significantly reducing post-heat-treat runout.

Yes. We can mask selected features with special masking compound to prevent carbon absorption in the masked area during carburizing — for example threads or areas requiring post-heat-treat machining. Share your print and stop-off requirements and we’ll confirm feasibility before quoting.

8620 contains nickel, chromium, and molybdenum, which give it predictable hardenability. When carburized, it forms an extremely hard outer wear layer (up to 62 HRC) while maintaining high core toughness to absorb shock loads. Maximum effective case depth achievable with 8620 is about 0.100” . When deeper case depths are required, a more hardenable carburizing alloy like 4320 or 9310 is required.

The concept of “effective” case depth is widely used in carburizing specs and part drawings, and refers to that part of the case that exceeds a defined limit, typically 50 HRC. So when a drawing specifies properties of 58-62 HRC to 0.050” depth, heat treaters interpret that as meaning the surface hardness must be between 58-62 HRC, and the case depth must be at or above 50 HRC to a depth of at least 0.050”. It is common also to see a specified range for effective case depth (for example 0.050 – 0.070”).
Total case depth is as it sounds – the depth at which case hardness decreases to core hardness.