Effective November 9th, 2026:

New Trucking Route Around Our Building. View the Route Here

Heat treating services

Age hardening / precipitation hardening

Age hardening (precipitation hardening) develops improved mechanical strength and impact toughness, in alloys like 17-4 PH. We routinely process material to standard industry tempers, including H900 and H1150 conditions.

Verify material condition

Solution Annealing Precedes Final Aging

Precipitation hardening must be performed on raw material or finish machined parts that are already in the solution-annealed state (Condition A). If your incoming bar stock requires solution treatment prior to aging, we coordinate the complete heat-treat cycle so your parts hit required drawing properties.

"*" indicates required fields

Name*

The final step, done right

Precision aging for finish-machined parts

Key advantages that make age hardening a low-risk final thermal step.

AMS 2750H certified uniformity

Furnaces designated for age hardening are calibrated and surveyed to strict temperature uniformity tolerances compliant with AMS 2759D specifications.

Predictable dimensional growth

Because aging operates at moderate temperatures without a severe liquid quench, dimensional movement remains minimal and predictable on finish-machined parts.

Reprocessing flexibility

If engineering callouts change, parts in lower aging conditions (like H900) can typically be re-aged to higher temper conditions (like H1150) without a full re-solution annealing cycle.

Age Hardening in Certified Furnaces

Why choose Thermex for age hardening

  • Multiple furnace sizes for batches large or small

    We run eight companion temper/aging furnaces (300-1,400°F operating range) for smaller precision valve trim, plus a dedicated pit-style furnace (48 inches in diameter, 96 inches deep, 500-1,200°F) for larger shaft production loads. All furnaces are regularly surveyed for temperature uniformity. Temperature Uniformity Survey (TUS) reports are available on request to satisfy your QA and audit requirements.
  • Built for oilfield & flow control alloys

    We regularly handle 17-4 PH and other precipitation-hardening grades used in high-pressure oilfield tools and valve assemblies.
  • Prototype testing & custom fixturing

    Beyond standard production runs, our team builds custom fixturing and develops specialized racking for prototype parts to ensure proper support across complex shapes.

Frequently Asked Questions

How much dimensional movement occurs during 17-4 PH age hardening?

Contraction occurs predictably during aging. For example, moving from Condition A to H900 results in a linear shrinkage of approximately 0.0004″ to 0.0006″ per inch. For most applications, age hardening can be performed on finished machined parts.

H900 uses a lower aging temperature (900°F) to yield peak tensile strength and hardness, but lower impact toughness. H1150 uses a higher temperature (1150°F), trading off some hardness for higher ductility and impact resistance.

To meet NACE requirements, the usual requirement is for double age hardening to 1150F (DH1150), a process which we regularly perform. If your application calls for certification to a sour-service or corrosion-resistant standard, share your print and spec requirements and we’ll confirm whether we can meet them before quoting.

We maintain temperature uniformity survey records and provide certified furnace charts and certificates of compliance detailing dwell times and setpoint temperatures. As well, thermocouple and controller calibration certificates are available on request.